Chlorinated Polyethylene PVC Impact Modifier CPE 135A CAS 63231-66-3
Phone Number : 18039110171 15638856372
WhatsApp : +8618039110171
Minimum Order Quantity : | 1 Ton | Price : | Negotiable |
---|---|---|---|
Packaging Details : | 25kg/woven bag | Payment Terms : | L/C, T/T, Western Union, MoneyGram |
Supply Ability : | 1000 Tons per month |
Place of Origin: | China | Brand Name: | RUNYE |
---|---|---|---|
Model Number: | CPE135A |
Detail Information |
|||
CAS No: | 63231-66-3 | Appearance: | White Powder |
---|---|---|---|
EINECS No.: | 203-052-4 | Tensile Strength: | ≥6.0Mpa |
The Number Of Colored Particles: | ≤60/100g | Volatile: | 0.75% |
Heat Of Fusion: | ≤ 2.0J/g | MF: | [CH2-CHCl-CH2-CH2]n |
Residueon Sieve(0.9mm): | ≤2.0% | Shore Hardness (A): | ≤64% |
Chlorine Content: | 35±1% | Density(25℃): | 1.24g/ml |
Highlight: | plastic toughener,chemical auxiliary agent |
Product Description
Cpe 135a For Pvc High Toughness White Powder Pvc Processing Aid Cas 63231-66-3 China Factory Price
Property:
CPE is odourless nontoxic and white or pale yellow powder with excellent resistance to weathering or age ozone chemicals, and good resistance to oil or flame. It is a colourable material with very good tenacity (flexible at -30 a brittle temperature under -70), and good miscibility with various polymers due to its properties of both plastics and rubber. CPE shows excellent resistance to very low temperature or high (a decomposition temperature above 160).
Use:
CPE has two series of thermoplastic resin and elastomer rubber. The thermoplastic CPE resin can be used alone to produce electric cable and waterproof roll etc. It also can be used as impact modifier blended with polyvinyl-chloride(PVC)polyethylene (PE) polypropylene(PP) polystyrene(PS) ABS or polyurethane(PU) etc. The elastomer CPE rubber shows both the elasticity of rubber and the resistance to oil chemicals heat cold and flame etc. Of plastics. The CPE as a special rubber with high performance can be used alone for rubber industry. It also can be used as modifier and solubilizer of general-purposed synthetic rubber blended with EPDM LIR NBR or CSM etc. So it can be used to produce flame retarded sheath of wire and cable conveyer belt rubber tubes waterproof roll rubber and seal with car etc.
Executive standard: HG/T 2704_2002
Technical specifications:
Item | Unit | Index |
Chlorine content 135A | % | 35±1 |
Heat of Fusion | J/g | ≤ 2.0 |
Tensile Strength | Mpa | ≥6.0 |
Residueon sieve(0.9mm) | % | ≤2.0 |
Shore Hardness (A) | % | ≤65 |
Elongation | % | ≥600 |
Density(25℃) | g/ml | 1.22 |
Mooney viscosity | ML(1+4) 125℃ | ≤96 |
The number of colored particles | 100g | ≤60 |
Volatile | % | 0.75 |
Packing:
25kg/bag or as customers' requirement