Purity White Powder YAXING Cas No 63231-66-3 PVC IMPACT MODIFIER
Phone Number : 18039110171 15638856372
WhatsApp : +8618039110171
Minimum Order Quantity : | 1 Ton | Price : | $ 700-$ 800 |
---|---|---|---|
Packaging Details : | 25kg/woven bag | Payment Terms : | L/C, T/T, Western Union, MoneyGram |
Supply Ability : | 1000 Tons per month |
Place of Origin: | China | Brand Name: | RUNYE |
---|---|---|---|
Model Number: | CPE135A |
Detail Information |
|||
Appearance: | White Powder | EINECS No.: | 203-052-4 |
---|---|---|---|
MF: | [CH2-CHCl-CH2-CH2]n | Chlorine Content: | 36±1% |
Density(25℃): | 1.23g/ml | Elongation: | ≥600% |
Heat Of Fusion: | ≤ 2.0J/g | Volatile: | 0.74% |
Tensile Strength: | ≥6.0Mpa | Residueon Sieve(0.9mm): | ≤2.0% |
Shore Hardness (A): | ≤65% | Mooney Viscosity: | ≤96ML(1+4) 125℃ |
The Number Of Colored Particles: | ≤60/100g | ||
Highlight: | chlorinated polyethylene rubber,chlorinated polyethylene powder |
Product Description
CPE 135A For PVC Bamboo And Wood Fiberboard High Grade Chlorinated Polyethylene PVC Processing Aid
Properties:
The product is no rules structure of the saturated thermoplastic resin, its appearance is white powder; it can be mixed and used with PVC, evidently increasing the impact resistance strength in lower temperature, flame resistance, ageing resistance and flexure performance.
CPE135A mainly used in products such as window profiles, pipes, pipefittings, extrusion board, and also used in magnetic materials, such as magnetic rubber strips and all type of flattened magnet.
Feature:
Excellent weather resistance, ozone resistance, chemical resistance and flame retardant, with a variety of plastics rubber has good compatibility
Effectively improve the toughness of rigid PVC products, anti-red and anti-aging properties,
Improve the melting point of PVC, has a good plasticizing properties.
Use:
CPE has two series of thermoplastic resin and elastomer rubber. The thermoplastic CPE resin can be used alone to produce electric cable and waterproof roll etc. It also can be used as impact modifier blended with polyvinyl-chloride(PVC)polyethylene (PE) polypropylene(PP) polystyrene(PS) ABS or polyurethane(PU) etc. The elastomer CPE rubber shows both the elasticity of rubber and the resistance to oil chemicals heat cold and flame etc. Of plastics. The CPE as a special rubber with high performance can be used alone for rubber industry. It also can be used as modifier and solubilizer of general-purposed synthetic rubber blended with EPDM LIR NBR or CSM etc. So it can be used to produce flame retarded sheath of wire and cable conveyer belt rubber tubes waterproof roll rubber and seal with car etc.
Technical specifications:
Item | Unit | Index |
Chlorine content | % | 35±1 |
Heat of Fusion | J/g | ≤ 2.0 |
Tensile Strength | Mpa | ≥6.0 |
Residueon sieve(0.9mm) | % | ≤2.0 |
Shore Hardness (A) | % | ≤65 |
Elongation | % | ≥600 |
Density(25℃) | g/ml | 1.22 |
Mooney viscosity | ML(1+4) 125℃ | ≤96 |
The number of colored particles | 100g | ≤60 |
Volatile | % | 0.75 |
Storage stability:
It should be stored in cool and dry places with good ventilation.